Caustics & Alkalis
Media Overview
Caustics & Alkalis — Media Overview
Caustic soda, potassium hydroxide, hypochlorite and kraft pulping liquors are strongly alkaline. They dissolve free silicon, attack fluoroelastomers when hot, crystallise when leakage meets air, and 50 % NaOH freezes at about +12 °C. A reliable caustic seal is built around these four behaviours rather than around the pump type. For production plants see Chlor-Alkali Plant, Alumina & Non-Ferrous Metals and Pulp & Paper Mill.
Key Sealing Challenges
- Free-silicon attack: reaction-bonded SiC loses its free silicon in hot caustic; only sintered (self-sintered) SiC is used.
- Atmospheric crystallisation: leakage absorbs CO₂ (2NaOH + CO₂ → Na₂CO₃ + H₂O) and forms hard crystals that hang up the faces; an API Plan 62 water or condensate quench washes them away.
- Freezing: 50 % NaOH solidifies near +12 °C; pump, seal chamber and quench lines are heat-traced.
- Elastomers: FKM degrades in hot caustic; EPDM (or FFKM at high temperature) is used.
- Caustic stress corrosion cracking: hot concentrated caustic can crack stressed stainless steel; nickel or high-nickel alloys are used above typical 316L limits.
Which mechanical seal is used on 50 % caustic soda pumps?
A balanced cartridge seal with sintered SiC vs sintered SiC faces (no reaction-bonded SiC), EPDM secondary seals and an API Plan 62 hot-water or condensate quench is typical, with Plan 11 on the process side. The pump and seal chamber are heat-traced to stay above the freezing point of 50 % NaOH.
Root-Cause Failure Analysis — Field Example
Symptom: 50 % caustic pump seal leaks after each shutdown; white crust on the gland.
├── Incorrect Response: "Tighten the gland and restart."
├── Diagnostic Evidence Required:
│ ├── Did the fluid in the seal chamber cool below about +15 °C?
│ ├── Is a quench fitted and flowing during start-up?
│ └── Are faces reaction-bonded SiC (free silicon)?
└── Engineered Solution:
├── Sintered SiC vs sintered SiC faces; EPDM O-rings.
├── API Plan 62 hot-water / condensate quench.
└── Heat-trace pump casing, seal chamber and quench lines.
Frequently Asked Questions
Why is EPDM preferred over Viton in caustic soda?
Fluoroelastomers (FKM / Viton) are attacked by hot alkalis and become hard and cracked. EPDM is resistant to caustic soda across the normal range of concentration and temperature.
Is a double seal needed for caustic?
Not usually. A single balanced seal with a Plan 62 quench is standard. A pressurised double seal is used for hot caustic above about 90 °C, for black liquor with solids, or where splashing would endanger personnel. Related: Chlor-Alkali Plant · Alumina · Pulp & Paper · Acids.
Request a Seal Selection
Send the fluid name and concentration, SDS, temperature, suction and discharge pressure, pump make and model, shaft size and speed to info@gipfelengg.com or use our enquiry form. Gipfel Engineering (ISO 9001:2015, NSIC-registered MSME, Mumbai) designs and manufactures mechanical seals, seal support systems and process pumps.
Equipment solutions: Overhung Pumps · Between-Bearings Pumps · Agitators.
Pump Duty & Mechanical Seal Selection Matrix
Typical values for selection guidance only. Final selection is made against the customer duty sheet and the fluid SDS.
| Pump duty | Fluid | Typical temp. | Typical pressure (bar) | Seal arrangement | Faces / elastomer | API piping plan |
|---|---|---|---|---|---|---|
| Caustic Soda Transfer Pump | NaOH 32 % | 30–60 °C | 3–6 bar | Balanced multi-spring cartridge | Sintered SiC vs sintered SiC / EPDM; 316L | API Plan 11 + Plan 62 water quench |
| Caustic Soda Pump, 50 % | NaOH 48–50 %, freezes ≈ +12 °C | 35–80 °C (heat-traced) | 3–8 bar | Balanced multi-spring cartridge | Sintered SiC vs sintered SiC / EPDM; 316L or nickel alloy | API Plan 11 + Plan 62 hot-water / condensate quench |
| Hot Caustic / Evaporator Pump | NaOH 50–70 % | 90–150 °C | 3–8 bar | Double cartridge, back-to-back (pressurised) | Sintered SiC vs sintered SiC / FFKM; nickel alloy | API Plan 53A |
| Potassium Hydroxide Pump | KOH 45–50 % | 30–80 °C | 3–6 bar | Balanced multi-spring cartridge | Sintered SiC vs sintered SiC / EPDM | API Plan 11 + Plan 62 |
| Sodium Hypochlorite Pump | NaOCl 10–15 % | Ambient | 2–4 bar | Balanced multi-spring cartridge | Sintered SiC vs sintered SiC / FKM; titanium metal parts | API Plan 11 |
| White / Green Liquor Pump | NaOH + Na₂S (+ Na₂CO₃, solids) | 80–100 °C | 3–6 bar | Balanced multi-spring cartridge | Sintered SiC vs sintered SiC / EPDM | API Plan 11 + Plan 62 |
| Black Liquor Pump | Concentrated black liquor, viscous | 90–130 °C | 3–8 bar | Double cartridge, back-to-back (pressurised) | Sintered SiC vs sintered SiC / EPDM or FFKM | API Plan 53A, or Plan 32 condensate flush |
Reviewed by Gipfel Engineering’s technical team.
Technical Information Disclaimer
The information on this page, including process descriptions, flow diagrams, operating ranges, seal arrangements, materials and piping plans, is general technical guidance for information only. Values shown are typical industry ranges, not guaranteed ratings or specifications of any Gipfel Engineering product. Each application differs. Seal selection, material compatibility, installation and operation must be verified by qualified personnel against the specific equipment data sheet, process conditions, applicable codes and the pump manufacturer’s instructions. A binding recommendation is given only in a written quotation or technical offer from Gipfel Engineering.
References to standards (such as API 682, ISO 21049, ISO 3069, FDA 21 CFR 177.2600 and NACE MR0175 / ISO 15156) describe common industry practice. They do not mean that any product is certified, qualified or approved to that standard unless this is confirmed in writing for a specific order. Third-party company and product names, including “equivalent to” references, are used for identification only and remain the trademarks of their owners. No affiliation, endorsement or OEM approval is implied.
Compliance with safety, hazardous-area, environmental and statutory requirements at the user’s site remains the responsibility of the plant owner or operator. To the extent permitted by law, Gipfel Engineering accepts no liability for loss or damage arising from reliance on this general information without a confirmed written recommendation. Content may change without notice.